search  current discussion  categories  materials - clay 

grolleg prices

updated sat 2 jan 10

 

mel jacobson on fri 1 jan 10


some have posted me off list that
in most parts of the country...grolleg is almost
twice the price of epk.

i did a quick check... just pound price.
i did not have a catalog.
mel
from: minnetonka, mn
website: http://www.visi.com/~melpots/
clayart link: http://www.visi.com/~melpots/clayart.html
new book: http://www.21stcenturykilns.com

Bryan Johnson on fri 1 jan 10


mel jacobson wrote:
> some have posted me off list that
> in most parts of the country...grolleg is almost
> twice the price of epk.
>
> i did a quick check... just pound price.
>
At 1000 pounds, a reasonable amount to buy at a time, for me at least,
the per pond prices from Continental are as follows.

EPK $0.33

English Grolleg (55# bag) $0.71

6 Tile Clay $0.27

Sure looks like Grolleg is more than twice the price.