Carissa Doying Cuny on tue 16 dec 97
Hi-
A mysterious glaze appeared in our lab. The name written on its
container is Egyptian Blue Raku. In The raku fire it turns out very dry,
light blue with blue speckles. I tried it at 04 in the electric kiln
and it became a watery blue. I have tested it over other glazes with
some really nice results. I would like to replicate this glaze but no
one here at Augusta State University knows where it came from. Does
anyone recognize this glaze? Thanks, Carissa, Chief Cook and Bottle
Washer of the Ceramics Lab
| |
|