another otto new turquoise for testing

updated mon 11 jan 10

 

lili krakowski on sun 10 jan 10


Second Otto New Turquoise


45.6 Feldspar--Kona F4
20.4 Strontium Carbonate
7.7 Bentonite
10.9 Copper Carbonate
10.9 Spodumene--Foote
5 Lithium Carbonate

100.5 Total


Unity Oxide
.27 Li2O
.169 Na2O
.077 K2O
.015 MgO
.044 CaO
.424 SrO
1.000 Total

.397 Al2O3
.011 Fe2O3

2.124 SiO2

5.4 Ratio
73.4 Exp

Comments:=3D20
Ok. So I should get a life! So in this cold where am I going to get one =
=3D
outside the house? Mmmmmm?

=3D20
-----------------------------------
Calculations by GlazeMasterT
www.masteringglazes.com
------------------------------------

Lili Krakowski
Be of good courage