I am lucky to live about 5 miles from a huge abandoned slab pile. There =
are hundreds of cords of pine and white spruce slabs. Also some edge trimmi=
ngs perfect for sidestoke wood.About 50 cords worth. I also have access to =
lots of pallets as it costs too much to ship them back South. My question-d=
o you guys burn them with the nails? Maybe a dumb question, but I have kept=
them out of my kiln because I wasn't sure about all that melting iron.

Claudia MacPhee Tagish, Yukon
www.paintedbyfire.blogspot.com