search  current discussion  categories  forms - misc 

s-cracks and drying platters.

updated sat 30 jan 10

 

Antoinette Badenhorst on fri 29 jan 10


S-cracks on the outside=3DC2=3DA0appear normally if the walls and basis are=
not=3D
of even thickness. That causes the clay to shrink uneven.=3D20

S-cracks on the inside is caused by water left on the inside and lack of co=
=3D
mmpression. Make sure to eliminate these mistakes and add to that the good =
=3D
advice as many has given. Let us know how it goes.=3D20



Antoinette Badenhorst=3D20
Lincolnshire, Illinois