Leon Popik on thu 18 dec 97
Would anybody have any experience with Shimpo Pugmills. I was thinking of
getting a Venco 3"de-airing but somebody mentioned Shimpo now has them. I
would like to hear if anybody has had any good/bad experiences with these
models.
Thanks in advance
Leon
Matthew Patton on fri 19 dec 97
Leon: I owned a Shimpo pugmill and had a generally bad experience with it.
For more details email me off list. M. Patton mjpat@msn.com
-----Original Message-----
From: Leon Popik
To: Multiple recipients of list CLAYART
Date: Thursday, December 18, 1997 6:16 AM
Subject: Shimpo pugmills
>----------------------------Original message----------------------------
>Would anybody have any experience with Shimpo Pugmills. I was thinking of
>getting a Venco 3"de-airing but somebody mentioned Shimpo now has them. I
>would like to hear if anybody has had any good/bad experiences with these
>models.
>
>Thanks in advance
>Leon
>
Frank Tucker on fri 19 dec 97
At 09:15 AM 12/18/97 EST, you wrote:
>----------------------------Original message----------------------------
>Would anybody have any experience with Shimpo Pugmills. I was thinking of
>getting a Venco 3"de-airing but somebody mentioned Shimpo now has them. I
>would like to hear if anybody has had any good/bad experiences with these
>models.
>
>Thanks in advance
>Leon
>
>
Hi Leon,
Shimpo will have a new pugmill available in January.It can be purchased with
or without the vacuum system which can be added later.I had the opportunity
to inspect and operate one and I was quite impressed.Your local Shimpo
dealer should have more information.
Frank Tucker