search  current discussion  categories  glazes - cone 4-7 

^6 reduction in clayart room

updated fri 19 mar 10

 

William & Susan Schran User on thu 18 mar 10


I plan on bringing samples of what we've been using/testing in ^6 reduction
at school to NCECA/Clayart room.
Last fall we made the switch from ^10 to ^6.

I'll also be there to answer questions about kiln shelves.

How many folks might be interested in looking at samples and discussing ^6
reduction?
When's a good time to meet?

Bill

--
William "Bill" Schran
wschran@cox.net
wschran@nvcc.edu
http://www.creativecreekartisans.com

Marcia Selsor on thu 18 mar 10


Bill,
I fired ^6 reduction for 20 years in Montana. I could contribute. My =3D
schedule is really getting full.
I maqde the switch in 1980.
Marcia Selsor
On Mar 18, 2010, at 11:59 AM, William & Susan Schran User wrote:

> I plan on bringing samples of what we've been using/testing in ^6 =3D
reduction
> at school to NCECA/Clayart room.
> Last fall we made the switch from ^10 to ^6.
>=3D20
> I'll also be there to answer questions about kiln shelves.
>=3D20
> How many folks might be interested in looking at samples and =3D
discussing ^6
> reduction?
> When's a good time to meet?
>=3D20
> Bill
>=3D20
> --
> William "Bill" Schran
> wschran@cox.net
> wschran@nvcc.edu
> http://www.creativecreekartisans.com
>=3D20

Marcia Selsor
http://www.marciaselsor.com