sharonia628 on sat 13 mar 10
All:
I should add to my earlier post about t.s. settling, that it is only the
white t.s. that settles. Probably the titanium dioxide I used to color it
with. Question remains, can I add something to it to keep it in suspension?
Thanks,
Sharon
| |
|