r type thermocoupler

updated mon 5 apr 10

 

David on fri 2 apr 10


I would like to ask if a "R" type thermocoupler will work with a J/K pyrome=
ter.
Thank you,
Dave
http://togeii.wordpress.com/

Steve Mills on fri 2 apr 10


I'm afraid the short answer is no.
You'd get a reading, but it would be *very* inaccurate!
J is calibrated for J only, likewise K, R, S, et al

You can get multi type Thermometers/Pyrometers, but they ain't cheap!

Steve M