I have used a simple clear recipe for a long time, but it gets cloudy in
any area that is thicker, and since I dip these carved platters, it isn't
suitable. Does anyone have a reliable, easy, transparent clear glaze for
firing at cones 6-9 that stays clear?? I would appreciate your help!
Thanks,
Joan
Joan Molloy Slack
Riverrun Center for the Arts
PO Box 95 6938 Bridge Road
McNaughton, Wi 54543
www.riverrunarts.com
715-277-4224
John Britt on tue 27 apr 10
What cone 6 or 9?