search  current discussion  categories  glazes - traditional iron glazes 

pumice celadon

updated mon 3 may 10

 

John Britt on wed 28 apr 10


Speaking of simple glazes...Here is a simple Celadon .

Celadon cone 10 reduction
80 Pumice (325 mesh)
20 Wollastonite


I posted an image and source for pumice (aka, volcanic ash)


http://ncclayclub.blogspot.com

John Britt
www.johnbrittpottery.com

Eric Hansen on thu 29 apr 10


nice - I just copied that to my desk top -

On Wed, Apr 28, 2010 at 10:36 AM, John Britt wr=
ote:

> Speaking of simple glazes...Here is a simple Celadon .
>
> Celadon cone 10 reduction
> 80 Pumice (325 mesh)
> 20 Wollastonite
>
>
> I posted an image and source for pumice (aka, volcanic ash)
>
>
> http://ncclayclub.blogspot.com
>
> John Britt
> www.johnbrittpottery.com
>