search  current discussion  categories  glazes - cone 04-06 

cone 06 repair question

updated mon 24 may 10

 

Marty Morgan on sun 23 may 10


I have a large bowl, glaze fired to cone 06, which was sitting at a slight
angle in the kiln and a piece of it stuck to the shelf above it. Is there
any way to fill in the missing bits and refire it? Generally my attitude
would be to toss it out, but it has a gorgeous painting done by a local
artist so I'd like to save it if possible. It was supposed to be in our
Empty Bowl silent auction. Our 10th Empty Bowl event had 1,053 people atten=
d
and raised $26,500 for the Food Pantry!

Marty Morgan, Gloucester, MA