updated thu 1 jan 98

 

J Rose Fine Pottery on wed 31 dec 97

Hi all!
Please help solve this mystery. Vase fired to cone 5 in oxidation, on
B-mix with an old reliable glaze now sweats. Customer returned it
because he couldn't put water in it and put it on his good furniture.
The glaze is not cracked or crackled and has been used on other pots
quite successfully. Any ideas?
June Rosenberry
Los Angeles