foam trimming batt making

updated sat 26 jun 10

 

jeanette harris on fri 25 jun 10


>Hi Randy,
>
>How are you trimming the bowls? I used to get cracks like that on my
>big bowls when I was securing the bowl onto the bat with little clay
>wads. When I switched to using a foam pad on top of a bat, the cracks
>disappeared. -snipping for bandwidth-
>
>Lynn

Hi,

If you want a detailed entry about how to make your own trim batts
with foam, go to my blog, http://www.jeanetteharrisblog.blogspot.com,
scroll down a few entries and there's a whole entry with photos of
how to make them. Any questions, please feel free to to ask.

Cheers,
Jeanette
--