Have you checked all of the thermocouple connections? I have an L&L. A co=
uple of times I got the E1 code when the set screw that holds one of the th=
ermocouple wires in place had worked loose. I really had to tighten it wel=
l to keep it from coming loose during the firing.

Alice DeLisle