Mike Gordon on sat 26 jun 10
Who wanted to know about this??
dansmith. com 800-4266740 1 gal $42.25 gum arabic. www.takachpress. com=3D2=
0=3D
=3DA0800-2483460 1 gal $34.00 gum arabic. Mike Gordon=3D
DJ Brewer on sat 3 jul 10
On 6/26/2010 4:08 PM, Mike Gordon wrote:
> Who wanted to know about this??
> dansmith. com 800-4266740 1 gal $42.25 gum arabic. www.takachpress.
> com 800-2483460 1 gal $34.00 gum arabic. Mike Gordon
I bought a gallon of gum arabic from Fuji film for $28. The number for
it is on my laptop. If someone wants it, email me and I'll give them
the number. I'm using it in this process of transfering photography to
leatherhard clay. You make your own ink using 2 teaspoons mason stain to
3 teaspoons linseed oil, stirred for about 15 to 20 minutes. It can be
fired to cone 10, provided the clay used is cone 10 clay. The gum arabic
is used on the paper photocopy to help the ink adhere to the toner on it.
http://ceramicartsdaily.org/ceramic-supplies/ceramic-colorants-ceramic-supp=
lies-2/photo-lithography-on-clay-a-surprisingly-simple-way-to-print-images-=
on-clay/
DJ
| |
|