Marcia Selsor on thu 1 jul 10


Begin forwarded message:

> From: Marcia Selsor
> Date: July 1, 2010 9:08:08 PM CDT
> To: Clyde Tullis
> Subject: Re: ITC application
>=3D20
> It is best sprayed on with a sand blaster. I use one hand on a drill =3D
stirring the ITC bucket and another aiming the sandblaster hooked up to =3D
my compressor.
> I thin coat is all you need. You must dilute the ITC 50% with the =3D
concentrate in the bucket as sold.
>=3D20
> Marcia Selsor
> http://www.marciaselsor.com
>=3D20
>=3D20
>=3D20
>=3D20

Marcia Selsor
http://www.marciaselsor.com