search  current discussion  categories  glazes - cone 8-10 

turning^10 glaze >^7

updated sun 4 jan 98

 

Mmpottery on sat 3 jan 98

Hi Everyone!
I feel like I should know this but I don't so here is the question;

I have a great ^10 salt glaze that I would like to lower to ^7. How
do I do this? Here is the recipe:
Super Salt ^10
Feldspar 1300 I haven't made this glaze in 15
years so I don't
Whiting 260 remember what feldspar. Any
hints would be
Tenn Ball 160 appreciated! I'm firing a new
salt kiln for the
Bentonite 40 first time! Thanks alot.
Michelle
Flint 200
Dolomite 40
Iron Ox 6%
Rutile 6%