Elaine Pinkernell on tue 3 aug 10
> I currently fire to cone 10 in a propane kiln but want to convert to
> firing electric to cone 5/6. I'm looking for a commercial glaze to
> use instead of my cone 10 Ohata. I don't expect to get the depth of
> color I get firing with gas but am more interested in finding a glaze
> that's a similar brick red that may break a bit on texture. Thx.
>
>
>
| |
|