Cathi Newlin on wed 11 aug 10
nds...)
I got some great feedback regarding my glaze tests last week and put it
all to use for my latest glaze firing.
Honestly, this is the first time in forever that I've not opened the
kiln only to want to chuck everything directly into the dry stream bed
next to the kiln!
I still have miles and miles to go, but I think I made real progress in
technique and in understanding how all this works.
If ya feel like having a look, yesterday's results are here:
http://squarepegarts.blogspot.com/2010/08/july-10-firing.html
As always, thanks for all the knowledge!
--
C Newlin