Hey Folks,=3D0A =3D0A It's taken about 5 days to get the moisture out and t=
he d=3D
raft is good so it's time to move the fire from the Pignose to the Bourry b=
=3D
ox...=3D0A=3D0Ahttp://www.youtube.com/watch?v=3D3DQiN8zmQvo_4=3D0A=3D0A I d=
ecided not=3D
to try for 1500=3DB0F with the Pignose.=3D0A =3D0AGary Navarre=3D0ANavarre=