Further down the digest Vince's post reminded me of teaching "short term"..=
. With only a month during winter to teach beginning ceramics drying became=
a priority. I solved it by putting wooden palettes under a large work tabl=
e, draping plastic down all 4 sides of the table, cut a hole in the plastic=
on the short end of the table to accommodate an electric heater. The heate=
r was the type that you can adjust the heat as well as the fan speed; turne=
d it all on high. I seem to recall that fresh pieces dried overnight. Can't=
remember if I weighted down the plastic at the bottom...
-Rimas