Arnold Howard on fri 1 oct 10


Several weeks ago there was a discussion on Clayart about
reusing underfired cones. It is an interesting topic, so I
test-fired 015 self-supporting cones to find out if
underfired cones would still be accurate. I discovered that
they bend just a little sooner than fresh cones. I posted a
picture comparing refired cones with fresh cones in
Paragon's Kiln Pointers newsletter:

http://www.paragonweb.com/Kiln_Pointer.cfm?PID=3D361

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / www.paragonweb.com