Alisa Liskin Clausen on sat 9 oct 10
Hi DJ
Now I have written to you, but will send this to Clay Art in case anyone
else is looking at these glaze tests.
I have corrected the Flickr site.
Since I am in in NJ and do have my glaze notes, I am comparing the photos o=
f
the glaze results and what I remember of these tests.
Whenever I do return to Denmark, I will double check, but I am almost
certain now what I write is correct.
I saw the Jeanie's Purple in Clay Times and noticed it is uses the same bas=
e
as MC6G Raspberry, with altered coloring oxides, I tested
the glaze and at some point saw the recipe for Raspberry Blue, also with th=
e
same base. I tested these the 3 glazes together, same base,
different colorants, to compare. So, the oxides were not properly deleted
from each test report.
Jeanies Purple is the Rasp. Base
ADD
0.2 Chrome
3.8 Tin Ox.
0.6 Cobalt Ox.
Raspberry Blue is Rasp. Base
ADD
1.0 Cobalt Ox.
0. RIO
MC6G Raspberry
ADD
0.2 Chrome
7.5 Tin
Sorry for the confusion but really happy people like you use the test
results
and help me to correct any errors. Many thanks.
Best regards from Alisa
.
--
Alisa Liskin Clausen
Troldskovvej 42
DK 6200 Aabenraa
Denmark
(45) 20 24 66 40
| |
|