DJ Brewer on sat 9 oct 10
On 10/9/2010 8:56 AM, Alisa Liskin Clausen wrote:
> Jeanies Purple is the Rasp. Base
> ADD
> 0.2 Chrome
> 3.8 Tin Ox.
> 0.6 Cobalt Ox.
>
> Raspberry Blue is Rasp. Base
> ADD
> 1.0 Cobalt Ox.
> 0. RIO
>
> MC6G Raspberry
> ADD
> 0.2 Chrome
> 7.5 Tin
>
Alisa --
in your original recipe on flickr -- it says COBALT CARB not cobalt oxide!
Just wanted to mention it!
| |
|