Dinah Snipes Steveni on tue 12 oct 10


Temp: 1253 degree centigrade with 30 minute soak. Oxidizing atmosphere. Sor=
ry for omitting this info. Test. Test. Test. Your body, your kiln, your hea=
t work, your ramps, your cool down, your raw materials.


Dinah