search  current discussion  categories  glazes - cone 4-7 

glossy brown cone 6 glaze/albany slip sub.

updated sat 23 oct 10

 

Alisa Liskin Clausen on fri 22 oct 10


Hi Tig,
Now I found some notes.

Lili's Albany sub.
580 Redart
80 Dolomite
25 Whiting

to add up to 100 gr. I made it
85 Redart
11 Dolomite
4 Whiting

I use Oldenwalder, a red clay, instead of Redart clay.

Best regards, from Alisa in Denmark

--
Alisa Liskin Clausen
Troldskovvej 42
DK 6200 Aabenraa
Denmark
(45) 20 24 66 40
www.alisapots.dk