search  current discussion  categories  techniques - decals 

fw: color decals

updated thu 16 dec 10

 

Susan Felts on wed 15 dec 10


Frank is right.... I have used this (http://www.easyceramicdecals.com ) =3D
online service to make wonderful decals.=3D20

If you can use Photoshop or know someone who does, you can load up a =3D
11x14" page with images, and they will make a decal sheet for you for =3D
$25 a page, and you can cut them out and soak in water to loosen them =3D
and then slide on your pots. They tell you exactly the temp to fire... =3D
somewhere close to 1800... It's been a while since I did it. The guy's =3D
name there is Andy Brayman, so I noticed you had tried a search for that =
=3D
name and come up empty. For $35 they will colorcheck your file and =3D
reprint if there are surface blemishes. Might be worth it if it's your =3D
first attempt. Color from a monitor and printing is a different animal. =
=3D
Hope this helps.=3D20

Susan Felts