John Post on thu 30 dec 10


I recently fired a currie grid using one of the Jun glaze recipes from
Mike Bailey's book as the basis for the fluxes in corner C. I came up
with an interesting fat white glaze that looks good over irony clay
bodies. If you fire at cone six and are interested, here's the link...

http://www.johnpost.us/Pottery%20Links/Test%20Tiles/posts-jun.html