John Post on thu 20 jan 11
I recently fired an Ian Currie grid of Glossy Base 1 from Mastering
Cone 6 Glazes by John Hesselberth and Ron Roy. Glaze number 17 on the
grid worked best over my RO-20 iron bearing clay from Rovin's Ceramics.
I tested glaze 17 from the grid with 9 different colorants which
yielded 45 different color variations.
You can see the grid glazes here...
http://www.johnpost.us/Pottery%20Links/grid-glazes/glossy-base-1.html
You can see the color variations here...
http://www.johnpost.us/Pottery%20Links/Test%20Tiles/glossy-base-test-tiles/=
glossy-base-tiles.html
John Post
Sterling Heights, Michigan
http://www.johnpost.us
Follow me on Twitter
https://twitter.com/UCSArtTeacher
| |
|