It is a complex question because the different locations had different =3D
types of clays. The proto porcelain I referred to in my post about =3D
Persians inspired to seek an opaque white glaze was taken from history =3D
not particularly concerned about kiln sites.
The proto porcelain was probably one of the light gritty clays mentioned =
=3D
in this link.

http://www.koh-antique.com/history/historytang5dynasty.htm

Marcia


On Jan 24, 2011, at 12:54 PM, rickmahaffey@comcast.net wrote:

> Dear Marcia,=3D20
>=3D20
>=3D20
>=3D20
> Thank you for the information! I missed your talk at NCECA Las Vegas. =
=3D
I was attending another presentation that was not as informative as =3D
yours!=3D20
>=3D20
>=3D20
>=3D20
> On the proto porcelain what date to you have for porcelain production =3D
in China? Visiting China I saw Museum displays indicating that proto =3D
porcelain was left behind by about 200 CE for the most part. What do =3D
you consider to be true porcelain? What is true porcelain and when it =3D
was in production is an interesting topic and there seem to be many =3D
differing opinions about that.=3D20
>=3D20
>=3D20
>=3D20
> Rick =3D20

Marcia Selsor
http://www.marciaselsor.com