search  current discussion  categories  materials - frits 

frits formulas

updated wed 21 jan 98

 

Tony Hansen on wed 14 jan 98

Does anyone know what frit 154, 146, 156 are? They are mentioned
on page 106 of last month's Ceramics Monthly. I have been watching
and I don't think anyone else has asked this.

--
-------
T o n y H a n s e n thansen@digitalfire.com
Get INSIGHT, Magic of Fire at http://digitalfire.com

Louis on tue 20 jan 98

Tony,
The only frit I could find with those numbers are
GF 146 by Gloster [(page 239)percent by weight]

K2O 1.00
Na2O 16.40
CaO 0.30
ZnO 4.20
Al2O3 23.90
B2O3 54.20
Source:
Advanced Ceramic Manual, Technical Data for the Studio Potter
by John W. Conrad, PhD; Falcon Company Publishing Division; copyright
1987.
Closest Frit equivalent is Ferro Frit 210R, on page 241.
Frit 154 and 156 I couldn't find.
good luck!
-Louis
Tony Hansen wrote:
> ----------------------------Original message----------------------------
> Does anyone know what frit 154, 146, 156 are? They are mentioned
> on page 106 of last month's Ceramics Monthly. I have been watching
> and I don't think anyone else has asked this.
>
> --
> -------
> T o n y H a n s e n thansen@digitalfire.com
> Get INSIGHT, Magic of Fire at http://digitalfire.com