search  current discussion  categories  glazes - cone 8-10 

request for pinnell red orange cone 10 or so reduction glaze

updated thu 10 feb 11

 

Veena Raghavan on tue 8 feb 11


Hi folks,

A request for help. Someone in our studion (Lee Arts Center in Arlington)
mixed what she called Pinnell Red Orange. She has since left and did not
leave the recipe. Since it was mixed for the studio, it should be there but=
is
not! Does anyone know of any such recipe? If so, I would really appreciate =
it
if you could post it. I have Pete's Cranberry, but this is obviously a
different glaze.

Thanks so much in advance.

Veena

VeenaRaghavan@cs.com

John Britt on wed 9 feb 11


Venna,

Posted it on the blog:

http://ncclayclub.blogspot.com

or you can now Google "Pete's Red Orange glaze recipe" and find it on th=
=3D
e blog.

Johnbrittpottery.com

Dannon Rhudy on wed 9 feb 11


Yes. You can get that recipe from Clay Times,
Pete's column of a while back....he did a series
on copper reds. That was one of the recipes
he gave. You can no doubt get the recipe, but
I highly recommend that you get hold of the articles.
I believe that there were three in that series.
Very edifying. I liked all three of the recipes,
but the orange-red is the most striking, on a white
claybody.

regards

Dannon Rhudy



-----Original Message-----
From: Clayart [mailto:Clayart@LSV.CERAMICS.ORG] On Behalf Of Veena Raghavan
Sent: Tuesday, February 08, 2011 9:24 PM
To: Clayart@LSV.CERAMICS.ORG
Subject: Request for Pinnell Red Orange Cone 10 or so Reduction Glaze

Hi folks,

A request for help. Someone in our studion (Lee Arts Center in Arlington)
mixed what she called Pinnell Red Orange. She has since left and did not
leave the recipe. Since it was mixed for the studio, it should be there but
is
not! Does anyone know of any such recipe? If so, I would really appreciate
it
if you could post it. I have Pete's Cranberry, but this is obviously a
different glaze.

Thanks so much in advance.

Veena

VeenaRaghavan@cs.com

Veena Raghavan on wed 9 feb 11


Thanks so much, John.

Clayart folk are amazing. I just knew that someone would come through.

As always, you are very generous in sharing. I have been enjoying your mini
videos too.

Thanks so much. Hope all is well.

Spring is around the corner. Yeah!

Warm regards.

Veena

VeenaRaghavan@cs.com