search  current discussion  categories  materials - misc 

more on wax

updated wed 16 feb 11

 

Rimas VisGirda on tue 15 feb 11


The old green wax I used in the 80's is NOT the green wax carried by Contin=
ental Clay. The old green wax was a similar formulation to Ceramul-A and wo=
uld not sustain freezing. It outperformed the no longer available Ceramul-A=
with the quirk that it needed prolonged drying time to reach its optimum r=
esistive qualities. It was carried and distributed by Aftosa, I was told th=
at Aftosa put the green color in to distinguish it from the other waxes tha=
t were being offered at the time. I have not tried the new green wax, so ha=
ve no feedback about its capabilities. -Rimas