MS AND K on thu 15 jan 98
Hi Group,
I'm a new potter, and a new computer user, with a few evening
courses and many flustrating hours labouring in the basemen under my bett. It
looks like it's paying off though, as I'm finally beginning to enjoy this!
I'm looking for a literature reference on stains and how to mix them into a
clay body and how to use them for surface decoration. If you know of a good
book or have any advice, I'd appreciate a response.
Thanks,
Kathy, Toronto
Valice Raffi on fri 16 jan 98
>----------------------------Original message----------------------------
Kathy wrote:
> I'm looking for a literature reference on stains and how to mix them into
>>a clay body and how to use them for surface decoration. If you know of
>>good book or have any advice, I'd appreciate a response.
Hi Kathy,
For surface decoration, try
"A Potter's Palette" by Christine Constant & Steve Ogden
Chilton ISBN: 0-8019-8753-9
Valice
in rainy Sacramento
DONPREY on sat 17 jan 98
In a message dated 1/16/98 6:11:57 AM, you wrote:
> I'm looking for a literature reference on stains and how to mix them into
>>a clay body and how to use them for surface decoration. If you know of
>>good book or have any advice, I'd appreciate a response.
>>
Kathy,
for mixing into clay bodies see "Finding One's Way with Clay" by Paulus
Berensohn. This was recently republished.
Don Prey in Oregon
Stephen Mills on sat 17 jan 98
This is a brilliant book!
Steve
Bath
UK
In message , Valice Raffi writes
>----------------------------Original message----------------------------
>>----------------------------Original message----------------------------
>Kathy wrote:
>> I'm looking for a literature reference on stains and how to mix them into
>>>a clay body and how to use them for surface decoration. If you know of
>>>good book or have any advice, I'd appreciate a response.
>
>
>Hi Kathy,
>
>For surface decoration, try
>
>"A Potter's Palette" by Christine Constant & Steve Ogden
>Chilton ISBN: 0-8019-8753-9
>
>Valice
>in rainy Sacramento
>
--
Steve Mills
Bath
UK
home e-mail: stevemills@mudslinger.demon.co.uk