Robert Fournier has a lovely mix of approximately 50/50 light machine
oil and candle wax. Once melted together it can be kept fluid in a hot
water bath, allows flowing resist decoration, & doesn't fry your brushes
(which can be cleaned with washing-up liquid). The only down side is the
waxed surface stays softish which makes it a bit frail.