clay body for tile

updated thu 24 feb 11

 

Maynard Leeman on tue 22 feb 11


Ben Gilliam uses a simple clay body for archeticual ceramics. I think h=
=3D
e fires to=3D20
about cone cone 1 but it will go much higher. It is a simple recepie.

equal parts of

fire clay Hawthorn=3D20
ball clay om4 ball clay
medium grogg

he uses it for making tiles and all kinds of stuff. I have used it to t=
=3D
hrow with.
I think you can use it for raku also.

its real simple, get a bag of each mix it up and you are ready to go.=3D20=
=3D
=3D20

no brainer.

Ron Roy on wed 23 feb 11


This body will fire to cone 10 but will also be loaded with
cristobalite - not a good component if making kitchen ware.

It will also leak at all cones between 1 and 10.

RR


Quoting Maynard Leeman :

> Ben Gilliam uses a simple clay body for archeticual ceramics. I
> think he fires to
> about cone cone 1 but it will go much higher. It is a simple recepie.
>
> equal parts of
>
> fire clay Hawthorn
> ball clay om4 ball clay
> medium grogg
>
> he uses it for making tiles and all kinds of stuff. I have used it
> to throw with.
> I think you can use it for raku also.
>
> its real simple, get a bag of each mix it up and you are ready to go.
>
> no brainer.
>