May Luk on tue 1 mar 11
Hello all;
I made this glaze test tile before but I didn't like it. Now I might
need this color for a job.
It is teal green with gold speck glaze (with a slow cool schedule) It
was a high alkaline dolomite glaze base. (HA13 or HA14 in cone 6 glaze
with Michael Bailey)
To make the TEAL color, is the colorant cobalt or copper? Titanium too?
Thanks in advance
May
Brooklyn NY
--
http://twitter.com/MayLuk
http://www.takemehomeware.com/
| |
|