glaze bubbles and runny, help!! please!

updated sun 13 mar 11

 

John Britt on sat 12 mar 11


Lisa,

My guess is you need to control your application (thinner) and fire slowe=
=3D
r (last 90=3D20
minutes) or soak it just under peak temperature.=3D20

You just need to apply the green thinner because when it combines with th=
=3D
e beige glaze they run (eutectic).

John Britt