search  current discussion  categories  techniques - cracking 

follow-up: plates cracking during bisque fire- success!

updated tue 3 may 11

 

Kristina Chadwick on mon 2 may 11


Thank you to everyone who responded to the post about my plates cracking
half during the bisque fire. I took all your suggestions and fired some n=
=3D
ew
plates. I put pieces of bisqued clay in between plates to allow for heat
flow and only stacked two plates high. Sweet success!

Thanks again for all your advice, I am so thankful to have access to the
collective expertise of the Clayart members.

Kristina