I just received 60 burrs, 30 40grit and 30 240grit, for $10.99 and $3.95 sh=
ipping on eBay. Came within 3-4 days. Haven't tried them yet, I very rarely=
need to grind anything and have an assortment of bits, probably SiC that I=
acquired when I got the Dremel (maybe 20-25 years ago). I'll try the new b=
its next time I need to grind... -Rimas