Suchman ceramics on fri 1 jul 11
Hi all,
I'm firing a great (to me) redware body that matures at ^1-3. I would
like a white slip that matches and fits well. The primary ingredient
in the body is Redart.
Any suggestions?
Thanks, Eric
--
-e-in-o'side-
pagan by nature
>http://www.flickr.com/photos/42169721@N04/
John Post on sat 2 jul 11
Lee posted this slip on clayart a while ago and it has worked well for
me at cone 1 over terra cotta clay.
Nepheline syenite 50
Kentucky OM #4 20
EPK 20
Flint 10
John
| |
|