mel jacobson on sun 3 jul 11
the stools i am making are for the farm.
we all sizes and shapes of people using the wheels
at the farm...and, they often use a lawn chair.
god awful.
so. this is not for me. and, i cannot think of
buying six stools @ $80 each.
so.
i am making quick and easy stools for group throwing.
tony:
if soda ash is the issue...take three pounds and put
it in a plastic bag, insert in pot. ship it.
when you get there...put the soda ash in hot
water...melt it. (microwave it.)
slather to taste over pots...soda ash reduction.
easy as pie.
mel
from: minnetonka, mn
website: http://www.visi.com/~melpots/
clayart link: http://www.visi.com/~melpots/clayart.html
new book: http://www.21stcenturykilns.com
alternate: melpots7575@gmail.com
| |
|