Lili Krakowski on thu 28 jul 11


I fire a manual electric kiln, not a digital one...and have never done =3D
much controlled cooling.
Nevertheless I have several white glazes I like.

Having said that: I find the absolutely nicest white glazes are =3D
dolomitic, with a combo of titanium, tin, and zirconium. Worth =3D
triaxials.

Same idea as chocolate cake with raspberries, Cointreau, and whipped =3D
cream: three paths to sheer bliss applied to Heaven.