DJ Brewer on thu 4 aug 11
To Vince Pitelka:
I have an "all purpose" slip base recipe of yours. Can it be used for
midrange firings as well as cone 10 firings? I'm assuming "yes" since it
says all purpose. I just want a simple slip recipe that I can put on
some bisqueware to give it a white slip coating.
Here is the recipe
EPK -- 34
OM4 -- 20
G-200 20
3134 frit 5
silica -- 21
zircopax -- 8
thanks in advance.
| |
|