search  current discussion  categories  techniques - stains 

white underglaze?

updated mon 8 aug 11

 

Judy Smith on sat 6 aug 11


I have several things I need to coat with white underglaze. Does anyone
have a recipe for white cone 6 oxidation underglaze. It is pretty expensiv=
e
to buy it in the little jars.

Thanks,
Judy Smith

raya hizi on sun 7 aug 11


Hi Judy,
I am using porcelain as white underglaze
Raya Hizi
Tel Aviv

On Sun, Aug 7, 2011 at 12:18 AM, Judy Smith wrote:

> I have several things I need to coat with white underglaze. Does anyone
> have a recipe for white cone 6 oxidation underglaze. It is pretty
> expensive
> to buy it in the little jars.
>
> Thanks,
> Judy Smith
>

Lee on sun 7 aug 11


Can you buy your clay store's white body dry? I use Super White
from Continental Clay as my white slip. It also fluxes at a low temp
and is good for flashing in soda and woodfire.

On Sat, Aug 6, 2011 at 4:18 PM, Judy Smith wrote:
> I have several things I need to coat with white underglaze. =3DA0Does any=
on=3D
e
> have a recipe for white cone 6 oxidation underglaze. =3DA0It is pretty ex=
pe=3D
nsive
> to buy it in the little jars.
>
> Thanks,
> Judy Smith
>



--=3D20
--
=3DA0Lee Love in Minneapolis
http://mingeisota.blogspot.com/

=3DA0"Ta tIr na n-=3DF3g ar chul an tI=3D97tIr dlainn trina ch=3DE9ile"=3D9=
7that is, =3D
"The
land of eternal youth is behind the house, a beautiful land fluent
within itself." -- John O'Donohue