Eleanora Eden on wed 10 aug 11
Hi Randy and Gregory and all,
I used CC165 and just made do with the brownish cast until I was at
Cherry Creek fair and Jonathan Kaplan came by and complained about
my icky brownish black.
So then I went half and half with CC165 and CC119. The 119 has a
bluish cast but the two together cancel each other out and I get
a real true black.
Best,
Eleanora
>Try Duncan Cover Coat CC165 Black Brown. Produces a matte black at cone ^6=
.
--
Bellows Falls Vermont
www.eleanoraeden.com
| |
|