J Motzkin on fri 12 aug 11
Hi, to what cone do you fire this clay? (It lists as a wide ranging cone 4-=
8
)
Oxidation or reduction?
Thanks
jmotzkin
@motzkin.com
-sent from my phone-
Pottery by John on fri 12 aug 11
I have used Standard Brooklyn Red and fired to Cone 6 oxidation and had goo=
d
results from the clay body. I also had no glaze fit issues with my regular
glazes. My one issue was that under my regular clear it did not maintain th=
e
red color but went brown. That defeated my intent with marbling it with
white and a tan clay for a nice red.
John Lowes
Sandy Springs, Georgia
http://wynhillpottery.weebly.com/
----- Original Message -----
From: "J Motzkin"
To:
Sent: Friday, August 12, 2011 9:31 AM
Subject: Brooklyn red
> Hi, to what cone do you fire this clay? (It lists as a wide ranging cone
> 4-8
> )
> Oxidation or reduction?
> Thanks
>
> jmotzkin
> @motzkin.com
> -sent from my phone-
| |
|