Lili Krakowski on sun 14 aug 11
Going down memory lane,..I actually liked that song "Diamonds and Rust."
Can't afford the first...but as to the latter.
Plain old rust makes nice speckles...well worth a try.
Dry out that steel wool pad disintegrating in the kitchen soap =3D
dish--just ignore the soap-- and pulverize it...Not too much just =3D
so....Test in a high magnesium glaze opacified with titanium...Nice.
You also can crawl under the vee-hickle armed with a steel brush and get =
=3D
some of that rust (wear safety goggles when steel brushing. ) Or, in =3D
case your pickup is as old as mine, just break a rusty bit off the body =3D
and pound it down to crumbs....
Just remember_rutile is titanium plus iron.
Lili Krakowski
Be of good courage
| |
|