Suchman ceramics on tue 13 sep 11
I was wondering if anyone could tell me the "recipe" for casting slip with
redart. I heard it was basically complete casting clay as it is. I was
wondering how much water and sodium silicate would be added? or Darvan?
Thanks all,
- Eric
-e-in-o'side-
pagan by nature
>http://www.flickr.com/photos/42169721@N04/
>http://www.etsy.com/shop/SalamanderStudios?ref=3Dsi_shop
John Britt on wed 14 sep 11
Here you go:
http://ncclayclub.blogspot.com/2010/03/casting-slip-cone-05.html
johnbrittpottery.com
| |
|